Crednerite Diffraction data computed using the structure from the paper listed below, along with the cell parameters refined from single crystal data of R070404 Topfer J, Trari M, Gravereau P, Chaminade J P, Doumerc J P Zeitschrift fur Kristallographie 210 (1995) 184-187 Crystal growth and reinvestigation of the crystal structure of crednerite, CuMnO2 Locality: synthetic CELL PARAMETERS: 5.5620 2.8820 5.8900 90.000 104.400 90.000 SPACE GROUP: C2/m ATOM X Y Z OCCUPANCY ISO(B) Cu 0.00000 0.50000 0.50000 1.000 0.861 Mn 0.00000 0.00000 0.00000 0.960 0.403 Cu 0.00000 0.00000 0.00000 0.040 0.403 O 0.40700 0.00000 0.17890 1.000 0.505 X-RAY WAVELENGTH: 1.541838 BOUNDS ON TWO THETA: 0.0 90.0 LIMITS IMPOSED ON THE INDICES ARE: +/- 4 +/- 2 +/- 5 MAX. ABS. INTENSITY / VOLUME**2: 59.69199171 The INTENSITY cut off value is 1.00 2-THETA INTENSITY D-SPACING H K L 31.36 51.46 2.8525 0 0 2 33.06 4.73 2.7098 -2 0 1 33.26 77.57 2.6936 2 0 0 35.32 10.54 2.5412 1 1 0 37.00 100.00 2.4297 -1 1 1 39.91 20.98 2.2588 -2 0 2 40.52 43.07 2.2263 1 1 1 44.90 1.07 2.0187 -1 1 2 47.83 2.23 1.9017 0 0 3 52.18 19.12 1.7529 2 0 2 56.98 30.46 1.6162 -1 1 3 59.37 29.13 1.5567 -3 1 1 64.56 21.10 1.4435 1 1 3 64.69 10.71 1.4410 0 2 0 65.44 6.29 1.4262 0 0 4 66.06 9.26 1.4143 -2 0 4 66.79 8.75 1.4006 3 1 1 69.36 5.31 1.3549 -4 0 2 69.84 3.98 1.3468 4 0 0 70.57 8.83 1.3347 -3 1 3 73.65 6.85 1.2862 0 2 2 74.71 10.10 1.2706 2 2 0 78.78 4.65 1.2148 -2 2 2 84.38 1.87 1.1479 2 0 4 86.09 3.77 1.1294 -4 0 4 87.44 3.78 1.1155 4 0 2 87.67 6.25 1.1131 2 2 2 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.