Megawite Zhao J, Ross N L, Angel R J Physics and Chemistry of Minerals 31 (2004) 299-305 Tilting and distortion of CaSnO3 perovskite to 7 GPa determined from single-crystal X-ray diffraction Note: P = 3.94 GPa Locality: synthetic _database_code_amcsd 0018609 CELL PARAMETERS: 5.4676 5.6267 7.8186 90.000 90.000 90.000 SPACE GROUP: Pbnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 240.536 Density (g/cm3): 5.709 MAX. ABS. INTENSITY / VOLUME**2: 123.7666407 RIR: 7.059 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 22.68 47.78 3.9212 1 1 0 4 22.75 22.45 3.9093 0 0 2 2 25.41 1.62 3.5051 1 1 1 8 31.81 25.30 2.8133 0 2 0 2 32.34 100.00 2.7685 1 1 2 8 32.76 22.89 2.7338 2 0 0 2 38.26 1.52 2.3526 1 0 3 4 38.37 1.68 2.3457 2 1 1 8 39.46 3.66 2.2835 0 2 2 4 40.25 3.87 2.2403 2 0 2 4 41.61 1.38 2.1705 1 1 3 8 46.31 26.39 1.9606 2 2 0 4 46.46 14.37 1.9547 0 0 4 2 47.83 1.11 1.9017 2 2 1 8 51.51 8.09 1.7741 1 3 0 4 52.19 11.69 1.7526 2 2 2 8 52.30 10.17 1.7494 1 1 4 8 52.80 4.24 1.7338 3 1 0 4 52.92 1.96 1.7301 1 3 1 8 57.00 17.31 1.6155 1 3 2 8 57.40 10.93 1.6052 0 2 4 4 58.00 10.46 1.5900 2 0 4 4 58.21 23.07 1.5850 3 1 2 8 66.47 2.93 1.4067 0 4 0 2 67.69 12.78 1.3842 2 2 4 8 68.66 2.82 1.3669 4 0 0 2 71.25 2.58 1.3236 0 4 2 4 71.87 5.05 1.3137 1 3 4 8 72.29 1.36 1.3071 3 3 0 4 72.93 2.85 1.2971 3 1 4 8 73.38 1.98 1.2903 4 0 2 4 76.10 2.88 1.2508 2 4 0 4 76.91 6.01 1.2396 3 3 2 8 77.13 7.48 1.2366 1 1 6 8 77.66 3.10 1.2295 4 2 0 4 80.65 3.31 1.1913 2 4 2 8 81.38 1.15 1.1824 0 2 6 4 81.90 1.12 1.1763 2 0 6 4 82.19 2.80 1.1728 4 2 2 8 84.94 2.60 1.1418 0 4 4 4 86.98 2.74 1.1202 4 0 4 4 88.76 1.73 1.1022 1 5 0 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.