Teallite Diffraction data computed using the structure from the paper listed below, along with the cell parameters refined from the powder pattern for R050434 Sejkora J, Berlepsch P, Makovicky E, Balic-Zunic T, Litochleb J Neues Jahrbuch fur Mineralogie, Abhandlungen 177 (2002) 163-180 Teallite from Radvanice near Trutnov (Czech Republic) Sample: Isotropic refinement Locality: Radvanice near Trutnov, Czech Republic CELL PARAMETERS: 11.35891 4.064086 4.274409 90.00000 90.00000 90.00000 SPACE GROUP: Pnma X-RAY WAVELENGTH: 1.541838 2-THETA INTENSITY D-SPACING H K L 22.19 39.07 4.0005 1 0 1 26.06 53.22 3.4152 2 0 1 26.94 82.09 3.3051 2 1 0 30.31 47.76 2.9453 0 1 1 31.34 100.00 2.8510 1 1 1 31.47 65.96 2.8397 4 0 0 31.53 7.41 2.8343 3 0 1 38.64 2.51 2.3278 4 1 0 38.69 45.67 2.3248 3 1 1 42.24 3.38 2.1372 0 0 2 43.02 20.22 2.1004 1 0 2 44.26 28.94 2.0443 4 1 1 44.54 25.33 2.0320 0 2 0 45.15 10.38 2.0061 5 0 1 48.75 21.70 1.8659 1 1 2 48.89 14.36 1.8612 3 0 2 50.31 8.30 1.8117 1 2 1 50.70 20.12 1.7988 5 1 1 52.34 13.67 1.7463 2 2 1 52.84 6.12 1.7310 6 0 1 53.33 11.61 1.7161 6 1 0 53.62 2.49 1.7076 4 0 2 54.15 10.72 1.6922 3 1 2 55.56 21.61 1.6525 4 2 0 55.60 2.88 1.6515 3 2 1 59.31 5.37 1.5566 5 0 2 63.07 1.64 1.4726 0 2 2 63.66 10.56 1.4604 1 2 2 63.99 10.67 1.4537 5 1 2 65.30 5.86 1.4276 5 2 1 65.63 5.50 1.4213 7 1 1 65.70 4.36 1.4199 8 0 0 66.02 1.71 1.4137 1 0 3 67.74 4.61 1.3820 2 0 3 68.27 8.90 1.3725 3 2 2 69.89 6.88 1.3446 0 1 3 70.14 1.02 1.3404 8 1 0 70.56 1.42 1.3335 3 0 3 71.53 4.01 1.3177 2 3 0 71.53 4.17 1.3177 6 2 1 72.19 1.68 1.3073 4 2 2 73.23 2.68 1.2914 0 3 1 73.16 3.30 1.2924 7 0 2 73.78 5.71 1.2831 1 3 1 74.05 3.89 1.2790 8 1 1 77.11 4.17 1.2357 5 2 2 77.42 1.88 1.2316 7 1 2 78.12 4.12 1.2223 3 3 1 78.66 8.41 1.2152 4 1 3 79.03 2.12 1.2104 9 0 1 81.87 3.42 1.1755 4 3 1 82.87 3.88 1.1639 8 2 0 83.20 2.38 1.1601 9 1 1 83.16 1.54 1.1605 1 2 3 84.75 4.30 1.1427 2 2 3 85.15 3.16 1.1384 1 3 2 85.15 2.05 1.1384 6 0 3 86.64 3.04 1.1227 5 3 1 87.39 1.39 1.1149 3 2 3 88.71 2.02 1.1017 6 3 0 89.37 1.92 1.0953 3 3 2 89.51 1.99 1.0940 10 1 0 89.87 3.43 1.0905 7 2 2 89.87 3.43 1.0905 7 2 2 XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.